1.The metal reflet glaze samples were prepared with the Huxian wheat-meal-stone accession 0%, 5%, 10% and 15% according to the traditional metal reflet glaze formula and then sintered at 950%.
1.摘金属光泽釉配方基础上,制作了4组
县麦饭石添量为0%,5%,10%,15%的金属光泽釉试
,
950℃
度环境下烧成。